Pool coating —
decorative, elastic, long-lasting
pool Pool coating

Pool coating —
decorative, elastic, long-lasting

Elastic protective and decorative coating for concrete swimming pools — UV-stable, with smooth easy-to-clean surface. Suitable as an additional protective layer over existing primary waterproofing. Direct on prepared concrete, no specialist pool contractor needed.

01 / The problem

Why pool coatings fail

Ein Pool ist eine der härtesten Anwendungen überhaupt — permanente Wasserlast, Chemikalien, UV. Falsches Material wird in 2–3 Saisons unbrauchbar. Die Sanierung kostet ein Vermögen, wenn die Fachfirma kommen muss.

water_drop

Hydrostatic pressure

Wasser drückt mit Gewicht — bei 2 m Tiefe schon 200 g/cm². Klassische Pool-Anstriche lösen sich an der Tieflinie zuerst, dann zieht sich das Problem nach oben. Die Beschichtung blättert in Streifen ab.

biotech

Chlorine attacks classic enamels

Freies Chlor (0,5–3 mg/l Standard für Schwimmbäder) ist ein starkes Oxidationsmittel. Standardlacke werden angegriffen, verfärben sich, werden brüchig. Nach 1–2 Saisons sind Risse und Verfärbungen sichtbar.

biotech

Algae infestation & green pool

Mikrofeine Risse oder raue Oberfläche bieten Algen Halt. Einmal etabliert, lassen sie sich kaum entfernen — der Pool wird grün, das Wasser muss komplett ausgetauscht werden. Glatte, dichte Oberfläche ist Pflicht.

02 / Why RubberPaint

Why liquid rubber for pools

shield

Suitable with standard pool care

Geeignet bei üblicher Pool-Pflege (freies Chlor < 1,5 mg/l, pH 6,8–8,2). Auch in salzelektrolyse-betriebenen Pools mit gepflegter Wasserchemie. Bei aggressiven Chemikalien oder permanenter Überchlorung: Beschichtung kann angegriffen werden.

vertical_align_bottom

Protective layer over primary waterproofing

Elastische Acryl-Beschichtung als zusätzliche Schutz- und Dekorschicht über vorhandener, ordnungsgemäß ausgeführter primärer Beckenabdichtung. Folgt thermischen Bewegungen des Untergrunds ohne zu reißen.

cleaning_services

Smooth surface

Algen finden keinen Halt. Reinigung mit Pool-Bürste und Standard-Reiniger problemlos — keine raue Struktur, in der sich Schmutz festsetzt.

wb_sunny

UV-stable, no embrittlement

Auch im Sommer in direkter Sonne flexibel und elastisch. Anders als klassische Pool-Anstriche, die unter UV-Belastung brüchig werden und nach 3 Jahren ersetzt werden müssen.

03 / Application

Step-by-step guide

Schritt 01 / 05

Empty and clean the pool

A dry substrate is essential.

Pool vollständig entleeren, abtrocknen lassen (mind. 7 Tage bei Sonnenwetter). Mit Hochdruck­reiniger Algen, Kalk und alte Beschichtungs­reste entfernen. Lose Stellen mechanisch lösen, Risse > 1 mm mit Beton-Reparatur­mörtel verschließen, 7 Tage aushärten lassen.

Empty and clean the pool
Schritt 02 / 05

Prime with deep-penetrating primer

Stabilise absorbent pool concrete.

Pool-Beton ist nach Reinigung stark saugend. Tiefengrund auftragen, 24 h trocknen lassen. Dies reduziert Verbrauch der ersten Schicht und verbessert Haftung. Bei Pools mit alter, defekter Beschichtung: bis aufs Beton entfernen, dann grundieren.

Prime with deep-penetrating primer
Schritt 03 / 05

First coat — penetration

Diluted with up to 5 % water (up to 10 % with airless sprayer).

Pinsel und Lammfellrolle. Verbrauch 200–250 g/m² (Pool-Beton ist sehr saugend). Auf Übergängen Boden-Wand, an Einlauf-Düsen und Skimmer-Anschlüssen besonders sorgfältig. Lückenlose Deckung — Pool-Beschichtung muss perfekt sein.

First coat — penetration
Schritt 04 / 05

Second coat — sealer

Undiluted after 24 h of drying.

Unverdünnt, kreuzweise zur ersten Schicht. Verbrauch 150–200 g/m². Trocknen lassen bis volldicht — bei Pool­anwendung mindestens 8 h, ideal über Nacht.

Second coat — sealer
Schritt 05 / 05

Third coat — deep line + jets

Reinforcement for high-load zones.

Dritte Schicht an Tieflinie (untere 60 cm), Übergängen zu Düsen, Skimmer und Treppen. Verstärkt die belastetste Zone, verhindert Ablösungen an Schlüsselpunkten. Verbrauch 100–150 g/m². Komplett aushärten lassen — 14 Tage minimum vor Wasser­befüllung, 28 Tage für volle Belastbarkeit.

Third coat — deep line + jets
lightbulb
Pro tip

Pool coating requires three coats instead of the usual two. Apply the third coat especially in the deep line and at inlet/outlet jets. Fill with water no earlier than 14 days after full curing, ideally after 28 days. IMPORTANT: RubberPaint is intended as an additional protective and decorative coating — a suitable primary pool waterproofing must already be professionally installed.

04 / Specifications

Technical data

Total consumption (3 coats) 0.5–0.6 kg/m²
Recommended coats 3 (deep line + jets)
Drying time 2 h dust-dry · 8 h recoatable
Curing before water filling 14–28 days
Full cure 28 days
Use case Decorative and protective layer over existing primary waterproofing
Recommended water quality free chlorine < 1.5 mg/l, pH 6.8–8.2 (standard pool care)
Binder note Acrylic-latex coating — not suitable for aggressive chemicals
Elasticity highly elastic (Class A0/C0 to EN 1062-1)
Service temperature −20 °C to +50 °C
Binder Acrylic latex (solvent-free)
05 / Material calculator

How much do I need?

Pools need 3 coats due to hydrostatic pressure. Calculate the interior area: floor + (perimeter × depth) + steps.

Standard: 3 Schichten. Pool-Standard.

info

Verbrauch: 170 g/m² pro Schicht. +10 % Reserve für Schnittkanten und unebene Flächen. Bei Großprojekten (> 80 m²) kontaktieren Sie uns für eine individuelle Beratung.

Empfehlung

6,6 kg benötigt

für 20 m² · 2 Schichten

Wird berechnet…

Gesamtmenge
Gesamtpreis

Versandkostenfrei ab 199 € — schauen Sie sich Ihren Warenkorb nach dem Hinzufügen an.

06 / Bestsellers

Empfohlene Farben für Pools

Hellblau und Dunkelblau lassen Wasser klarer und tiefer wirken — Pool-Klassiker. Hellgrün für tropische Optik, Weiß für maximale Helligkeit, Grau für moderne Architektur-Pools.

08 / FAQ

FAQ — pool coating

Kann ich über alte Pool-Beschichtung auftragen?
Nur wenn die alte Beschichtung 100 % tragfähig ist — was bei alten Pools selten der Fall ist. Empfehlung: alte Beschichtung mechanisch komplett entfernen (Sandstrahlen oder Bohrhammer mit Spachtel), bis auf festen Beton. Dann Tiefengrund, dann RubberPaint in 3 Schichten. Halbe Sachen ruinieren das Ergebnis und kosten doppelt.
Wann darf ich den Pool wieder mit Wasser füllen?
Frühestens nach 14 Tagen Aushärtung, ideal nach 28 Tagen. Bei früherem Befüllen erreicht die Beschichtung nicht ihre volle Festigkeit und kann unter Wasserdruck versagen. Geduld zahlt sich aus — eine Saison mehr warten ist deutlich günstiger als eine Komplett-Sanierung.
Wie lange hält die Beschichtung bei intensiver Nutzung?
Bei sachgerechter Anwendung und normaler Pool-Pflege: viele Saisons. Wichtig: pH-Wert im üblichen Pool-Standardbereich (6,8–8,2) halten, Chlor unter 1,5 mg/l (übliche Pflege-Empfehlung), Algen­bildung frühzeitig bekämpfen. Jährliche Sichtprüfung beim Wassertauschen, Reparaturstellen punktuell nachbeschichten — verlängert Lebensdauer drastisch.
Funktioniert es auch bei Salzelektrolyse-Pools?
Ja, RubberPaint ist auch für Salzelektrolyse-Pools geeignet. Salz selbst ist kein Problem — die durch Elektrolyse erzeugten Chlor­spitzen können kurzzeitig höher liegen als bei Standardchlorung. Wichtig: regelmäßige Chlor­messung, bei Spitzen über 5 mg/l Wassermenge erhöhen oder Elektrolyse-Leistung reduzieren.
Kann ich Whirlpool oder Spa-Bereich beschichten?
Whirlpool ja, aber mit Einschränkung: Temperaturen über +40 °C dauerhaft können die Beschichtung beanspruchen. Beim regelmäßigen Whirlpool-Betrieb (38–40 °C) hält RubberPaint zuverlässig. Bei Spa mit höheren Temperaturen (z. B. Sauna-Tauchbecken mit Wechseltemperaturen): vorher mit unserem Support-Team Materialempfehlung abstimmen.

Got a technical question about pool coating?

Unser Team berät Sie zu Pool-Vorbereitung, Materialbedarf und Aushärtungszeiten — kostenlos und unverbindlich.